Wieland 1925 Wilaform Palladium

Category Metal , Nonferrous Metal , Precious Metal , Palladium Alloy , Pure Element
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1925 Wilaform Palladium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine palladium in standard purity.Applications: chains, pipesDental
Physical Properties Metric English Comments
Density 12.0 g/cc
0.434 lb/in³
Thermal Properties Metric English Comments
Melting Point 1555 °C
2831 °F
Component Elements Properties Metric English Comments
Palladium, Pd 99.95 %
99.95 %
Descriptive Properties Value Comments
Color grey