Williams Advanced Alloys WS157 Solder

Category Metal , Nonferrous Metal , Indium Alloy , Solder/Braze Alloy , Pure Element
Manufacturer Williams Advanced Alloys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS157 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.96 MPa
575 psi
Thermal Properties Metric English Comments
CTE, linear 24.8 µm/m-°C

@Temperature 20.0 °C
13.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 82.0 W/m-K
569 BTU-in/hr-ft²-°F
Melting Point 157 °C
315 °F
Solidus 157 °C
315 °F
Liquidus 157 °C
315 °F
Component Elements Properties Metric English Comments
Indium, In 100 %
100 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00003071 ohm-cm
0.00003071 ohm-cm