Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.50 g/cc
0.307 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.5 MPa
7610 psi
Thermal Properties Metric English Comments
CTE, linear 21.6 µm/m-°C

@Temperature 20.0 °C
12.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 49.0 W/m-K
340 BTU-in/hr-ft²-°F
Melting Point 183 - 188 °C
361 - 370 °F
Solidus 183 °C
361 °F
Liquidus 188 °C
370 °F
Component Elements Properties Metric English Comments
Lead, Pb 40 %
40 %
Tin, Sn 60 %
60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001496 ohm-cm
0.00001496 ohm-cm