Material Notes:
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided by Aurora Technologies.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 110
110
Tensile Strength, Ultimate 138 MPa
20000 psi
Flexural Strength 159 MPa
23000 psi
Compressive Strength 262 MPa
38000 psi
Shear Strength 82.7 MPa
12000 psi
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
Mechanical
140 °C
284 °F
Electrical
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+13 ohm-cm
3.00e+13 ohm-cm
Surface Resistance 7.00e+11 ohm
7.00e+11 ohm
Dielectric Constant 4.9

@Frequency 1e+6 Hz
4.9

@Frequency 1e+6 Hz
Dielectric Strength 18.7 kV/mm
475 kV/in
Dielectric Breakdown 65000 V
65000 V
Dissipation Factor 0.042

@Frequency 1e+6 Hz
0.042

@Frequency 1e+6 Hz
Arc Resistance 124 sec
124 sec
Descriptive Properties Value Comments
Color Natural