Material Notes:
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers excellent machineability and chemical resistance. Standard color is ivory. Black and blue are available upon request.Zellamid® 1100 is ideally suited for heavy duty plastic components and offers many advantages in comparison with steel: corrosion resistance, low weight, and low wear - e.g. for crane sheaves or carriage wheels for ropeways which are produced as finished parts by spin casting.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Moisture Absorption at Equilibrium 2.5 - 3.0 %
2.5 - 3.0 %
Saturation at 50% RH
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 83 - 85
83 - 85
DIN 53505
Ball Indentation Hardness 163 MPa
23600 psi
DIN 53456
Tensile Strength at Break 88.0 - 90.0 MPa
12800 - 13100 psi
DIN 53455
Elongation at Break 10 - 40 %
10 - 40 %
DIN 53455
Tensile Modulus 3.90 GPa
566 ksi
DIN 53457
0.800 GPa

@Temperature 100 °C
116 ksi

@Temperature 212 °F
DIN 53457
Charpy Impact Unnotched NB
NB
DIN 53453
Charpy Impact, Notched 2.50 - 3.00 J/cm²
11.9 - 14.3 ft-lb/in²
DIN 53453
Coefficient of Friction 0.050 - 0.10
0.050 - 0.10
to steel, added lubrication
0.30 - 0.35
0.30 - 0.35
to steel, no lubrication; ISO/DTR 7147
Abrasion 82
82
mm³; DIN 53516
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.67 J/g-°C
0.399 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long time operation
120 - 140 °C
248 - 284 °F
medium time operation
160 °C
320 °F
a few hours operation
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Permissible Unit Pressure 25 - 30 MPa
Time yield limit up to 5
s1/1000; DIN.53444