Material Notes:
HyTemp 4052 contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance with good low temperature.Improved low-temperature properties with slightly less oil resistance than 4051 types. Excellent compression set.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 32 - 40

@Temperature 100 °C
32 - 40

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.50 %
<= 0.50 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -32.0 °C
-25.6 °F
Gehman T100
Glass Transition Temp, Tg -32.0 - -25.3 °C
-25.6 - -13.5 °F
Zeon Test #1273
Descriptive Properties Value Comments
% Volume Swell 17
Curesite Dual
Gel-Mek (%), max 10
Heat Loss (%) Max 0.7