Zeon Chemicals Nipol® 1000x132 Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 1000x132 Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol 1000X132 is a copolymer of butadiene and acrylonitrilewith extremely high fuel and oil resistance. Sufficient antioxidant is added duringmanufacture for normal storage conditions.Ultra-high ACN level for maximum oil and fuel resistance and low gas permeability
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Mooney Viscosity 45 - 65

@Temperature 100 °C
45 - 65

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 1.0 %
<= 1.0 %
Zeon Test #873
Descriptive Properties Value Comments
AO Type SS
Bound ACN (%, acrylonitrile) 50-52
Heat Loss (%) Max 1
Hot/Cold C