Zeon Chemicals Nipol® 1022x59 Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 1022x59 Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol 1022X59 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions. This product also has improved UV stabilization.Precrosslinked to provide low nerve and minimum die swell in extruded goods. Excellent as a compounding ingredient in PVC and ABS.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Mooney Viscosity 53 - 68

@Temperature 100 °C
53 - 68

@Temperature 212 °F
(1+4)
Ash <= 0.80 %
<= 0.80 %
Zeon Test #873
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 31-34
Gel-Mek (%) 75-85
Heat Loss (%) Max 0.5
Hot/Cold H