Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals Nipol® 1442 Nitrile Powder and Crumb Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 1442 Nitrile Powder and Crumb Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol 1442 is a copolymer of butadiene and acrylonitrile with medium-high acrylonitrile content. Nipol 1442 shall be in the form of nominal 1/4" three-dimensional chips containing approximately 5%mineral dusting agent to prevent agglomeration. It shall be free from foreign material considered objectionable for normal applications.Crumb rubber with talc partitioning agent. Used in coal tar and asphalt modification.
Physical Properties Metric English Comments
Particle Size 9500 µm
9500 µm
Viscosity 2000 - 10000 cP
2000 - 10000 cP
Unmilled Cement; Zeon Test #328
Mooney Viscosity 75 - 90

@Temperature 100 °C
75 - 90

@Temperature 212 °F
(1+4); Zeon Test #404
Ash 0.20 - 0.80 %
0.20 - 0.80 %
Zeon Test #873
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -35.0 - -25.0 °C
-31.0 - -13.0 °F
Descriptive Properties Value Comments
Bound ACN (%, acrylonitrile) 32-34
Heat Loss (%) Max 0.7
Hot/Cold C