Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer

Category Polymer , Thermoplastic , Cyclo Olefin Polymer
Manufacturer Zeon Chemicals
Trade Name Zeonex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zeonex®330R has a lower birefringence than other Zeonex® products. This grade can satisfy market demands in the optical area where low birefringence and high dimensional stability in precision optical parts is required.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Water Absorption <= 0.010 %
<= 0.010 %
Melt Flow 9.0 - 14 g/10 min

@Load 2.16 kg,
Temperature 280 °C
9.0 - 14 g/10 min

@Load 4.76 lb,
Temperature 536 °F
Z-011A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.001 MPa
4641.3 psi
Elongation at Yield 2.0 %
2.0 %
Tensile Modulus 1.80 GPa
261 ksi
Flexural Strength 66.0 MPa
9570 psi
Flexural Modulus 2.80 GPa
406 ksi
Izod Impact, Notched 0.108 J/cm
0.202 ft-lb/in
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 123 °C
253 °F
Optical Properties Metric English Comments
Refractive Index 1.509
1.509
Transmission, Visible 92 %
92 %