Zeon Chemicals Zeonor® 750R Cyclo Olefin Polymer

Category Polymer , Thermoplastic , Cyclo Olefin Polymer
Manufacturer Zeon Chemicals
Trade Name Zeonor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zeonor® 750R Cyclo Olefin Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation using proprietary technology for a wide range of electronic, automotive and packaging applications.Zeonor® can be processed for any of these applications via injection molding, blow molding or extrusion.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Water Absorption <= 0.010 %
<= 0.010 %
ASTM D570
Moisture Vapor Transmission 0.110 cc-mm/m²-24hr-atm
0.279 cc-mil/100 in²-24hr-atm
40°C, 90%, 50-300&#956m; JIS K7129
Melt Flow 27 g/10 min

@Load 2.16 kg,
Temperature 280 °C
27 g/10 min

@Load 4.76 lb,
Temperature 536 °F
JIS K 6719
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
ISO 527
Elongation at Break 140 %
140 %
ISO 527
Tensile Modulus 2.00 GPa
290 ksi
ISO 527
Flexural Strength 55.0 MPa
7980 psi
ISO 178
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648
Glass Transition Temp, Tg 70.0 °C
158 °F
JIS K7121
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 92 %

@Thickness 3.00 mm
92 %

@Thickness 0.118 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC250
Dielectric Constant 2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
IEC250
Dielectric Strength 70.0 kV/mm
1780 kV/in
ASTM D149
Dissipation Factor 0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
IEC250