Zeon Chemicals Zetpol® 2030H Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 2030H Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zetpol 2030H is a high-Mooney version of a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.Higher Mooney version of Zetpol 2030. Especially suited for dynamic oil field components. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Iodine Absorption Number 30 - 45
30 - 45
mg/100mg; R-133A
Mooney Viscosity >= 110

@Temperature 100 °C
>= 110

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Descriptive Properties Value Comments
% HYD 85
Bound ACN (%, acrylonitrile) 34.9-37.5
Heat Loss (%) Max 1