Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner 301-G0 Flammable Resistant

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner 301-G0 Flammable Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, Frameworks of Deflection Coils, Hi-Pressure Outputs Package, Plugs of Kinescopes Autos and Others: Ignition Systems, Heating Systems, Electricity Distribution Systems, Tail Lights Base, Shells of Ignition Coils, Door Handles, Air-Condition LatticesInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
D792
Water Absorption 0.10 %
0.10 %
23°C•24h; D570
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
D638
Flexural Strength 85.0 MPa
12300 psi
D790
Flexural Modulus 2.20 GPa
319 ksi
D790
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
IS0179
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
IS0179
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
D696
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
D257
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
D150
Dielectric Strength 19.0 kV/mm
483 kV/in
D149
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
D150
Processing Properties Metric English Comments
Processing Temperature 215 - 255 °C
419 - 491 °F
Nozzle Temperature 240 °C
464 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 120 - 130 °C

@Time 14400 sec
248 - 266 °F

@Time 4.00 hour
Injection Pressure 40.0 - 100 MPa
5800 - 14500 psi
3-15 sec
Back Pressure 4.00 - 15.0 MPa
580 - 2180 psi
Copyright © lookpolymers.com All Rights Reserved