Material Notes:
Applications: High Glossy PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
GB/1033
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
GB/15585
Melt Flow 3.0 g/10 min
3.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
GB/1040
Flexural Strength 50.0 MPa
7250 psi
GB/9341
Charpy Impact Unnotched NB
NB
IS0179-1:2000
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
GB1634
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
D257
Processing Properties Metric English Comments
Processing Temperature 165 - 250 °C
329 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 85.0 °C

@Time 10800 sec
185 °F

@Time 3.00 hour
Horizontal Oven
90.0 °C

@Time 7200 sec
194 °F

@Time 2.00 hour
Chute Hot-Wind
Injection Pressure 40.0 - 100 MPa
5800 - 14500 psi
Descriptive Properties Value Comments
Speed of Shoot, % 45-85