Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
GB/1033
Mechanical Properties Metric English Comments
Tensile Strength, Yield 67.0 MPa
9720 psi
GB/1040
Flexural Strength 116 MPa
16800 psi
GB/9341
Charpy Impact Unnotched NB
NB
IS0179-1:2000
Charpy Impact, Notched 1.04 J/cm²
4.95 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
GB1634
Flammability, UL94 V-0
V-0
GB/T2408
Electrical Properties Metric English Comments
Comparative Tracking Index 300 V
300 V
GB/4207
Processing Properties Metric English Comments
Processing Temperature 255 - 280 °C
491 - 536 °F
Mold Temperature 45.0 - 100 °C
113 - 212 °F
Drying Temperature 110 °C

@Time 7200 sec
230 °F

@Time 2.00 hour
Vacuum Pressure, -0.08 MPa
120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Chute Hot-Wind
120 °C

@Time 21600 sec
248 °F

@Time 6.00 hour
Horizontal Oven
Injection Pressure 35.0 - 100 MPa
5080 - 14500 psi
Descriptive Properties Value Comments
Speed of Shoot, % 35-80
Users viewing this material also viewed the following: