Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
GB/1033
Water Absorption 0.60 %
0.60 %
23°C•24h
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
GB/15585
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.0 MPa
13900 psi
GB/1040
Flexural Strength 134 MPa
19400 psi
GB/9341
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
IS0179-1:2000
Charpy Impact, Notched 0.660 J/cm²
3.14 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
GB1634
Flammability, UL94 V-0
V-0
GB/T2408
Flammability Test 12
12
Flame Remainder (%); GB/9345
Processing Properties Metric English Comments
Processing Temperature 255 - 280 °C
491 - 536 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 110 °C

@Time 10800 sec
230 °F

@Time 3.00 hour
Vacuum Pressure, -0.08 MPa
120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Chute Hot-Wind
120 °C

@Time 21600 sec
248 °F

@Time 6.00 hour
Horizontal Oven
Injection Pressure 50.0 - 100 MPa
7250 - 14500 psi
Descriptive Properties Value Comments
Speed of Shoot, % 35-90