Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner PC/ABSz-4 Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PC/ABSz-4 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
GB/1033
Water Absorption 0.30 %
0.30 %
GB/T1034
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
GB/15585
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
GB/1040
Flexural Strength 82.0 MPa
11900 psi
GB/9341
Charpy Impact Unnotched NB
NB
IS0179-1:2000
Charpy Impact, Notched 4.50 J/cm²
21.4 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
GB/1634
Flammability, UL94 HB - V-0
HB - V-0
GB/T2408
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
D257
Comparative Tracking Index 200 V
200 V
GB/4207
Processing Properties Metric English Comments
Processing Temperature 225 - 270 °C
437 - 518 °F
Drying Temperature 100 °C

@Time 14400 sec
212 °F

@Time 4.00 hour
Chute Hot-Wind
100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Horizontal Oven
Injection Pressure 50.0 - 100 MPa
7250 - 14500 psi
Descriptive Properties Value Comments
Chromatism (?E) =0.8
Granule Diameter Φ3x3-5
Speed of Shoot, % 35-80
Surface Polish High
Weatherability Adjustive
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved