Material Notes:
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Bulk Density 0.310 g/cc
0.0112 lb/in³
Loss On Ignition 5.0 %
5.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000660 GPa
0.0957 ksi
As Received, Parallel to thickness
0.000230 GPa

@Temperature 760 °C,
Time 86400 sec
0.0334 ksi

@Temperature 1400 °F,
Time 24.0 hour
Parallel to Thickness
Compressive Yield Strength 0.170 MPa
24.7 psi
at 10% Compression, Parallel to thickness
Thermal Properties Metric English Comments
Thermal Conductivity 0.0550 W/m-K

@Temperature 200 °C
0.382 BTU-in/hr-ft²-°F

@Temperature 392 °F
Parallel to Thickness
0.0550 W/m-K

@Temperature 200 °C
0.382 BTU-in/hr-ft²-°F

@Temperature 392 °F
0.110 W/m-K

@Temperature 600 °C
0.763 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.205 W/m-K

@Temperature 1000 °C
1.42 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Parallel to Thickness
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage 0.500 %

@Temperature 760 °C,
Time 86400 sec
0.500 %

@Temperature 1400 °F,
Time 24.0 hour
Perpendicular to Thickness
2.50 %

@Temperature 1000 °C,
Time 86400 sec
2.50 %

@Temperature 1830 °F,
Time 24.0 hour
Parallel to Thickness
3.50 %

@Temperature 1000 °C,
Time 86400 sec
3.50 %

@Temperature 1830 °F,
Time 24.0 hour
Perpendicular to Thickness
Component Elements Properties Metric English Comments
Al2O3 33 %
33 %
Other 1.0 %
1.0 %
Other Metal Oxides
5.0 %
5.0 %
Organic Content
SiO2 61 %
61 %
Electrical Properties Metric English Comments
Dielectric Strength 1.06 kV/mm
27.0 kV/in
Descriptive Properties Value Comments
Color Off White