Material Notes:
Zircar’s unique process for manufacturing yttria-stabilized zirconia cloths and felts is also used in the production of pure zirconia refractory fibers and textiles without stabilizers. For those processes which are intolerant of yttria, these unstabilized pure zirconia fiber products provide much of the same high performance insulating benefits. Pure zirconia fibers exist in the monoclinic crystal phase and appear white in color. Our high purity zirconia fiber and textiles are offered in six different standard product forms; bulk fiber Type ZOBF, two felts Types ZOF-50 and ZOF-100 and three types of knit cloth Types ZOK-15, ZOW-15 and ZOW-30.Features: High Purity ZirconiaHigh Temperature StabilityLow Thermal ConductivityExcellent Thermal Shock ResistanceNo OutgassingSix Different Product Formats OfferedAvailable ‘Off the Shelf’Application Information: Pure zirconia cloth is used as high temperature insulation for advanced energy systems.Information provided by Zircar Zirconia.
Physical Properties Metric English Comments
Loss On Ignition 0.340 %

@Temperature 950 °C,
Time 3600 sec
0.340 %

@Temperature 1740 °F,
Time 1.00 hour
Outgassing - Total Mass Loss 0.00 %
0.00 %
Thermal Properties Metric English Comments
Melting Point 2590 °C
4690 °F
Shrinkage 0.000 %

@Temperature 1650 °C,
Time 3600 sec
0.000 %

@Temperature 3000 °F,
Time 1.00 hour
Component Elements Properties Metric English Comments
CaO 0.040 %
0.040 %
HfO2 1.0 - 2.0 %
1.0 - 2.0 %
Na2O 0.020 %
0.020 %
SiO2 0.22 %
0.22 %
Y2O3 <= 0.0010 %
<= 0.0010 %
ZrO2 >= 97 %
>= 97 %