Zoltek Panex 30® High Twist Carbon Roving

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 30®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 30® High Twist Carbon Roving.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Twist Carbon RovingApplications include: Friction Clutches & Brakes, Composite Substructures
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1552 MPa
225100 psi
Tensile Modulus 221 GPa
32100 ksi
Component Elements Properties Metric English Comments
Carbon, C 99 %
99 %
Descriptive Properties Value Comments
Denier (g/9000m) 4820
Twist S
Z