Zotefoams ZOTEK® F 74 HT PVDF Foam

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Zotefoams
Trade Name ZOTEK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams ZOTEK® F 74 HT PVDF Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zotek® F 74 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Compliant with US FDA regulations.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0740 g/cc
0.00267 lb/in³
ISO 845
Cell Length 0.420 mm
0.0165 in
Mechanical Properties Metric English Comments
Hardness, Shore A 26
26
ISO 868
Hardness, Shore O 34
34
ISO 868
Hardness, Shore OO 82
82
ISO 868
Tensile Strength 1.411 MPa
204.6 psi
ISO 1798
Elongation at Break 132 %
132 %
Compressive Yield Strength 0.218 MPa

@Strain 25.0 %
31.6 psi

@Strain 25.0 %
ISO 7214
Tear Strength 1.48 kN/m
8.44 pli
ISO 8067
Compression Set 13.2 %

@Time 79200 sec,
Strain 50.0 %
13.2 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; ISO 7214
Thermal Properties Metric English Comments
Thermal Conductivity 0.0343 W/m-K
0.238 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
0.0390 W/m-K
0.271 BTU-in/hr-ft²-°F
mean temp of 50°C; ISO 8301
0.0441 W/m-K
0.306 BTU-in/hr-ft²-°F
mean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 160 °C
320 °F
Descriptive Properties Value Comments
Flammability Heat Release: FAR/CS 25.853
Pass at 1/2 in
Radiant Heat Panel: FAR 25.856
Pass at 1/8, 1/2, and 1 in
Smoke Density: ABD0031
Pass at 1/2 in
Smoke Density: FAR/CS 25.853
Pass at 1/2 in
Toxic Gas Emission: ABD0031
Pass at 1/2 in
Vertical Burner (60 sec): FAR/CS 25.853
Pass at 1 in