Material Notes:
Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Melt Flow 20 g/10 min
20 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.5 MPa
3410 psi
Elongation at Break 110 %
110 %
Flexural Modulus 1.52 GPa
220 ksi
Izod Impact, Notched 0.932 J/cm
1.74 ft-lb/in