Zylog Hipolyene® 6251 Y M2 Thermoplastic Polyolefin & PP Compound

Category Polymer , Thermoplastic , Polyolefin , Polypropylene (PP)
Manufacturer Zylog Plastalloys
Trade Name Hipolyene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Hipolyene® 6251 Y M2 Thermoplastic Polyolefin & PP Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Melt Flow 16 g/10 min
16 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.1 MPa
2770 psi
Elongation at Break 40 %
40 %
Flexural Modulus 1.91 GPa
277 ksi
Izod Impact, Notched 1.57 J/cm
2.94 ft-lb/in