Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zylog Neoplast® 180 C Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Zylog Plastalloys
Trade Name Neoplast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Neoplast® 180 C Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neoplast 180 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D 2240
86

@Treatment Temp. 150 °C,
Time 605000 sec
86

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 9.32 MPa
1350 psi
500 mm/min; ASTM D 412
10.3 MPa

@Treatment Temp. 150 °C,
Time 605000 sec
1490 psi

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 550 %
550 %
500 mm/min; ASTM D 412
495 %

@Treatment Temp. 150 °C,
Time 605000 sec
495 %

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00638 GPa
0.925 ksi
500 mm/min; ASTM D 412
Tear Strength 49.0 kN/m
280 pli
500 mm/min; ASTM D 624
Compression Set 48 %

@Temperature 70.0 °C,
Time 79200 sec
48 %

@Temperature 158 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Continuous; SAE J 2236
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D 746
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved