Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.000542 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.0100 - 0.0150 g/cc
0.000361 - 0.000542 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 65L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plasters with low thermal conductivity.Information provided by NOVA Chemicals...
Density 0.0100 - 0.0150 g/cc
0.000361 - 0.000542 lb/in³
Polimeri Europa Extir® LN 7000 Expandable Polystyrene
Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e..
Density 0.0100 - 0.0150 g/cc
0.000361 - 0.000542 lb/in³
Density range normally used
Polimeri Europa Extir® A 7000 Expandable Polystyrene, Standard  (discontinued **)
Particle size range is 1.5 - 2.2 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type A..
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 76L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plates with low thermal conductivity.Information provided by NOVA Chemicals.
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 76XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Production of low density blocks, recommended for the elastified plates after cutting..
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T163B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl..
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T263B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low density foam.Applications: This grade is used mainly for..
Density 0.0140 - 0.0150 g/cc
0.000506 - 0.000542 lb/in³
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene
General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and convent..
Density 0.0140 - 0.0150 g/cc
0.000506 - 0.000542 lb/in³
IRPC Polimaxx Pentfoam 355E Expandable Polystyrene
GENERAL: PENTFOAM "355E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST EXPANSION RATE AND S..