| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 2000 AE Expandable Polystyrene, Standard Flame Retardant
Particle size range is 0.4 - 75 mm. Minimum apparent density on a discontinuous pre-expander is 17 g/l.Processing technology used for Type A 2000 AE is: Molding, Traditional and Vacuum.Specific cha..
|
|||
| Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® B 3000 AE Expandable Polystyrene, Fast Molding Flame Retardant
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 17 g/l.Processing technology used for Type B 3000 AE is: Molding, Vacuum.Specific characteristics: DIN..
|
|||
| Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | Normal range, one pre-expansion |
|
SABIC EPS 452 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 452 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
|
|||
| Density | 0.0180 - 0.0400 g/cc | 0.000650 - 0.00145 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 45B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding of very thin parts (5 mm to 20 mm).Infor..
|
|||
| Density | 0.0180 - 0.0400 g/cc | 0.000650 - 0.00145 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from ..
|
|||
| Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC..
|
|||
| Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | |
|
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene
(discontinued **)
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad..
|
|||
| Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® B 3000 Expandable Polystyrene, Fast Molding
(discontinued **)
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 17 g/l.Processing technology used for Type B 3000 is: Molding, Vacuum.Specific characteristics: Good m..
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 323 FC Expandable Polystyrene
TPC - 323 FCApplications: faster cycling shape molding with wall thickness >10mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | molding density range |
|
IRPC Polimaxx Pentfoam 355E Expandable Polystyrene
GENERAL: PENTFOAM "355E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST EXPANSION RATE AND S..
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | molding density range |
|
IRPC Polimaxx Pentfoam 361F Expandable Polystyrene
GENERAL: PENTFOAM "361F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
|
|||
| Density | 0.0180 g/cc | 0.000650 lb/in³ | 2.4 minute residence time pre-expander |
|
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the..
|
|||
| Density | 0.0180 g/cc | 0.000650 lb/in³ | 1 minute residence time |
|
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..
|
|||
| Density | 0.0180 g/cc | 0.000650 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
|
Zotefoams Plastazote® LD18 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
|
|||
| Density | 0.0180 - 0.0240 g/cc | 0.000650 - 0.000867 lb/in³ | sheet density |
|
Zotefoams Plastazote® LD18SC Low Density Polyethylene Foam, Small Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
|
|||
| Density | 0.0180 - 0.0480 g/cc | 0.000650 - 0.00173 lb/in³ | |
|
BASF Styropor® BF 422 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
|
|||
| Density | 0.0180 - 0.800 g/cc | 0.000650 - 0.0289 lb/in³ | |
|
BASF Styropor® BFL 327 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..
|
|||
| Density | 0.0180 - 0.0650 g/cc | 0.000650 - 0.00235 lb/in³ | |
|
BASF Styropor® BFL 422 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 321 HS Expandable Polystyrene
TPC - 321 HSApplications: shape molding with wall thickness > 10 mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 326 WP Expandable Polystyrene
TPC - 326 WPApplications: low water absorption, longer cycling shape molding with wall thickness >10 mmInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0200 g/cc | 0.000650 - 0.000723 lb/in³ | |
|
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene
GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
|
|||
| Density | 0.0180 - 0.0200 g/cc | 0.000650 - 0.000723 lb/in³ | |
|
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene
GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA..
|
|||
| Density | 0.0180 g/cc | 0.000650 lb/in³ | 75 second cycle time |
|
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave..
|
|||
| Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | Normal range, one pre-expansion |
|
SABIC EPS 450FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 450FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
|
|||
| Density | 0.0180 - 0.0220 g/cc | 0.000650 - 0.000795 lb/in³ | |
|
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene
General: Pentfoam 328H is a high density grade expandable polystyrene containing pentane as blowing agent, this grade is developed to meet the demand for fast molding cycles in vacuum machineApplica..
|
|||