Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.000903 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0100 - 0.0250 g/cc
0.000361 - 0.000903 lb/in³
Polimeri Europa Extir® LN 5000 Expandable Polystyrene
Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e..
Density 0.0150 - 0.0250 g/cc
0.000542 - 0.000903 lb/in³
Normal range, one pre-expansion
SABIC EPS 650FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 650FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Density 0.0160 - 0.0250 g/cc
0.000578 - 0.000903 lb/in³
Normal range, one pre-expansion
SABIC EPS 652 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Density 0.0150 - 0.0250 g/cc
0.000542 - 0.000903 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 65XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informati..
Density 0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0100 - 0.0250 g/cc
0.000361 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® A 5000 Expandable Polystyrene, Standard  (discontinued **)
Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type A..
Density 0.0160 - 0.0250 g/cc
0.000578 - 0.000903 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova Styrocell® M442C Expandable Polystyrene
A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4..
Density 0.0130 - 0.0250 g/cc
0.000470 - 0.000903 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 121 HS Expandable Polystyrene
TPC - 121 HSApplication: low density blocksInformation provided by Iran Petrochemical Commercial Co.
Density 0.0140 - 0.0250 g/cc
0.000506 - 0.000903 lb/in³
molding density range
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene
General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure..
Density 0.0140 - 0.0250 g/cc
0.000506 - 0.000903 lb/in³
molding density range
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene
General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..
Density 0.0160 - 0.0250 g/cc
0.000578 - 0.000903 lb/in³
molding density range
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene
General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and convent..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD23 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..