| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 2000 AE Expandable Polystyrene, Standard Flame Retardant
Particle size range is 0.4 - 75 mm. Minimum apparent density on a discontinuous pre-expander is 17 g/l.Processing technology used for Type A 2000 AE is: Molding, Traditional and Vacuum.Specific cha..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 3000 AE Expandable Polystyrene, Standard Flame Retardant
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 AE is: Molding, Vacuum.Specific characteristics: DIN..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® B 5000 AE Expandable Polystyrene, Fast Molding Flame Retardant
Particle size range is 0.9 - 1.6 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type B 5000 AE is: Blocks.Specific characteristics: DIN 4102 c..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir® LN 3000 Expandable Polystyrene
Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Normal range, one pre-expansion |
|
SABIC EPS 550FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 550FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Normal range, one pre-expansion |
|
SABIC EPS 552 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 552 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 55B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fastmolding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Inform..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 55C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Infor..
|
|||
| Density | 0.0150 - 0.0300 g/cc | 0.000542 - 0.00108 lb/in³ | Pressurized batch pre-foamer; Usual Use |
|
NOVA Chemicals Gedexcel® 64XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks f average and low densities.Information..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **)
Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **)
Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
|
|||
| Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **)
Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 3000 Expandable Polystyrene, Standard
(discontinued **)
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 is: Molding, Traditional and Blocks.Specific charact..
|
|||
| Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® PD D 5000 AE Expandable Polystyrene, Fast Molding Flame Retardant
(discontinued **)<
Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 11 g/l. Minimum apparent density on a discontinuous pre-expander is 14 g/l. Minimum apparent density on a cont..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® IA 2000 Expandable Polystyrene, Special Purpose
(discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type IA 2000 is: Molding, Transfer.Specific characteristics: ..
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
|
Ineos Nova Styrocell® M544C Expandable Polystyrene
A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell is..
|
|||
| Density | 0.0150 - 0.0300 g/cc | 0.000542 - 0.00108 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
|
Ineos Nova T523C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly ..
|
|||
| Density | 0.0150 - 0.0300 g/cc | 0.000542 - 0.00108 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
|
Ineos Nova T543B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly ..
|
|||
| Density | 0.0140 - 0.0300 g/cc | 0.000506 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 221 HS Expandable Polystyrene
TPC - 221 HSApplication: low to medium density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 323 FC Expandable Polystyrene
TPC - 323 FCApplications: faster cycling shape molding with wall thickness >10mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | molding density range |
|
IRPC Polimaxx Pentfoam 355E Expandable Polystyrene
GENERAL: PENTFOAM "355E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST EXPANSION RATE AND S..
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | molding density range |
|
IRPC Polimaxx Pentfoam 361F Expandable Polystyrene
GENERAL: PENTFOAM "361F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
|
|||
| Density | 0.0250 - 0.0300 g/cc | 0.000903 - 0.00108 lb/in³ | ISO 845-88 |
|
Eurofoam Euroflex Art. 110 Polyurethane Foam
Information provided by Eurofoam s.r.l.
|
|||
| Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir® LN 2000 Expandable Polystyrene
Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 2000 Expandable Polystyrene, Standard
(discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 16 g/l.Processing technology used for Type A 2000 is: Molding, Traditional.Specific characteristics..
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 321 HS Expandable Polystyrene
TPC - 321 HSApplications: shape molding with wall thickness > 10 mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | Final Product Density |
|
Iran Petrochemical (PCC) TPC - 326 WP Expandable Polystyrene
TPC - 326 WPApplications: low water absorption, longer cycling shape molding with wall thickness >10 mmInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Density | 0.0180 - 0.0300 g/cc | 0.000650 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir Leonardo A 2000 AE Expandable Polystyrene
(discontinued **)
Extir A 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 200..
|
|||