| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum apparent density on a continuous pre-expander after two expansions |
|
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS 33MA Modified Expandable Polystyrene
Applications: Insulation, bean bags, SIP's, ICF'sInformation provided by NOVA Chemicals.
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS M77A Expandable Polystyrene Resin
Applications Insulation, Bean bag, SIP'sInformation provided by NOVA Chemicals
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS M77B Expandable Polystyrene Resin
Applications Insulation, SIP's, Fabricated PackagingInformation provided by NOVA Chemicals
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS M77B Modified Expandable Polystyrene
Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals.
|
|||
| Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum apparent density on a continuous pre-expander after two expansions |
|
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | |
|
Polimeri Europa Extir® LN 2001 Expandable Polystyrene
Extir LN 2001 belongs to a new expandable product family, the Leonardo Series. Extir LN 2001 is specially coated to be incorporated into bricks, concrete, mortar and plaster, in order to lighten the..
|
|||
| Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **)
Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
|
|||
| Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® PD D 5000 AE Expandable Polystyrene, Fast Molding Flame Retardant
(discontinued **)<
Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 11 g/l. Minimum apparent density on a discontinuous pre-expander is 14 g/l. Minimum apparent density on a cont..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
|
NOVA Chemicals Styrocell® B933A Expandable Polystyrene
(discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the ..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
|
Ineos Nova T163B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
|
Ineos Nova T243C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
|
Ineos Nova T263B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low density foam.Applications: This grade is used mainly for..
|
|||
| Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
|
Ineos Nova T733B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used after expansion for cellular bricks.Applications: This grade is..
|
|||
| Density | 0.0120 - 0.0130 g/cc | 0.000434 - 0.000470 lb/in³ | |
|
IRPC Polimaxx Pentfoam 155E Expandable Polystyrene
General: Pentfoam 155E is a self extinguising grad expandable polystyrene containing pentate as blowing agentApplications: Pentfoam 155E is particularly well suited for the manufacture of low densit..
|
|||
| Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | molding density range |
|
IRPC Polimaxx Pentfoam 155E Expandable Polystyrene
General: Pentfoam 155E is a self extinguising grad expandable polystyrene containing pentate as blowing agentApplications: Pentfoam 155E is particularly well suited for the manufacture of low densit..
|
|||
| Density | 0.0120 - 0.0130 g/cc | 0.000434 - 0.000470 lb/in³ | |
|
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene
General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..
|
|||
| Density | 0.0120 - 0.0130 g/cc | 0.000434 - 0.000470 lb/in³ | |
|
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene
General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar..
|
|||
| Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | molding density range |
|
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene
General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar..
|
|||
| Density | 0.0120 - 0.020 g/cc | 0.000434 - 0.00072 lb/in³ | expanded |
|
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding
High quality processingHigh strengthLow wasteFast moulding cycles
|
|||
| Density | 0.0120 g/cc | 0.000434 lb/in³ | 95 second cycle time |
|
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a..
|
|||
| Density | 0.0120 g/cc | 0.000434 lb/in³ | 127 second cycle time |
|
Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding
100% PolystyrenePre-expansionThis is the low pentane version for high quality block molding.Block MouldingJackocell® S2314 represents the favorite choice for the manufacture of high quality insul..
|
|||
| Density | <= 0.0120 g/cc | <= 0.000434 lb/in³ | TMA |
|
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta..
|
|||
| Density | <= 0.0120 g/cc | <= 0.000434 lb/in³ | TMA |
|
Akzo Nobel Expancel® 950 DU 120 Dry unexpanded microspheres