Polymer Property : Density = 0.0140 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.00900 - 0.0140 g/cc
0.000325 - 0.000506 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T443C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Density 0.0130 - 0.0140 g/cc
0.000470 - 0.000506 lb/in³
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene
General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure..
Density 0.0130 - 0.0140 g/cc
0.000470 - 0.000506 lb/in³
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene
General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..