| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 3000 AE Expandable Polystyrene, Standard Flame Retardant
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 AE is: Molding, Vacuum.Specific characteristics: DIN..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® B 5000 AE Expandable Polystyrene, Fast Molding Flame Retardant
Particle size range is 0.9 - 1.6 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type B 5000 AE is: Blocks.Specific characteristics: DIN 4102 c..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
|
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant
b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Normal range, one pre-expansion |
|
SABIC EPS 550FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 550FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS 33MAHD Modified Expandable Polystyrene
Applications: Insulation, board stockInformation provided by NOVA Chemicals.
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS 33MC Modified Expandable Polystyrene
Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals.
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
|
NOVA Chemicals EPS 34RC Regular Expandable Polystyrene
Applications: PackagingInformation provided by NOVA Chemicals.
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
|
NOVA Chemicals EPS 35MC Modified Expandable Polystyrene
Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals.
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS M77C Expandable Polystyrene Resin
Applications Insulation, SIP's, Fabricated Packaging/Fine SurfaceInformation provided by NOVA Chemicals
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
|
NOVA Chemicals EPS M77C Expandable Polystyrene Resin
Applications Insulation, SIP's, Fabricated Packaging/Fine SurfaceInformation provided by NOVA Chemicals
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
|
NOVA Chemicals EPS R244C Expandable Polystyrene Resin
Applications Thermal and Regular PackagingInformation provided by NOVA Chemicals
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
|
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
|
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
|
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
|
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
|
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **)
Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
|
|||
| Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 3000 Expandable Polystyrene, Standard
(discontinued **)
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 is: Molding, Traditional and Blocks.Specific charact..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | After expansion - see notes |
|
NOVA Chemicals Arcel 310 B 65% PS/35% PE Blue Interpolymer
(discontinued **)
Applications: Resilient/reusable packaging, Sports items, DunnageExpansion: Minimum Density Potential (pcf): Single pass continuous - 1.35; Double Pass continuous - 1.0; Batch expansion - 1.2Prepuff..
|
|||
| Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
|
Ineos Nova Styrocell® M442C Expandable Polystyrene
A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4..
|
|||
| Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
|
Ineos Nova Styrocell® M442C Expandable Polystyrene
A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4..
|
|||
| Density | 0.0160 g/cc | 0.000578 lb/in³ | 1.2 minute residence time pre-expander |
|
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
|
|||
| Density | 0.0160 g/cc | 0.000578 lb/in³ | 75 rpm |
|
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a..
|
|||
| Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
|
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
|
|||
| Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
|
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
|
|||
| Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
|
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
|
|||
| Density | 0.0160 g/cc | 0.000579 lb/in³ | Nominal |
|
Hexcel® HexWeb® CR III 3/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
|
|||
| Density | 0.0160 g/cc | 0.000579 lb/in³ | Nominal |
|
Hexcel® HexWeb® CR III 3/8-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
|
|||
| Density | 0.0160 - 0.0480 g/cc | 0.000578 - 0.00173 lb/in³ | |
|
BASF Styropor® BF 327 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
|
|||
| Density | 0.0160 g/cc | 0.000579 lb/in³ | Free Rise Density, 5% H<sub>2</sub>O |
|
ACC EP LS EPI Engineered Polymers Leak Stop MDI
EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will soli..
|
|||