| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | >= 0.0170 g/cc | >= 0.000614 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
|
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Normal range, one pre-expansion |
|
SABIC EPS 552 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 552 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 55B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fastmolding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Inform..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 55C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Infor..
|
|||
| Density | 0.0170 - 0.0350 g/cc | 0.000614 - 0.00126 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 55XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Usual Use |
|
NOVA Chemicals Gedexcel® 65B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of average to high density blocks and molding of the shape of bulky packaging and parts for the building industry.Informat..
|
|||
| Density | 0.0170 - 0.0350 g/cc | 0.000614 - 0.00126 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC..
|
|||
| Density | 0.0170 - 0.0350 g/cc | 0.000614 - 0.00126 lb/in³ | |
|
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **)
Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30..
|
|||
| Density | 0.0170 - 0.0350 g/cc | 0.000614 - 0.00126 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® PD D 3000 AE Expandable Polystyrene, Fast Molding Flame Retardant
(discontinued **)<
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 16 g/l. Minimum apparent density on a continuous pre-expander is 18 g/l.Processing technology used fo..
|
|||
| Density | 0.0170 g/cc | 0.000614 lb/in³ | 2.4 minute residence time pre-expander |
|
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
|
|||
| Density | 0.0170 g/cc | 0.000614 lb/in³ | 100 rpm |
|
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a..
|
|||
| Density | 0.0170 g/cc | 0.000614 lb/in³ | 1.5 minute residence time |
|
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..
|
|||
| Density | 0.0170 - 0.0290 g/cc | 0.000614 - 0.00105 lb/in³ | sheet density |
|
Zotefoams Plastazote® MP24 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 091 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 091 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 091 WUF 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 551 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 551 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 092 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | 0.0170 - 0.0800 g/cc | 0.000614 - 0.00289 lb/in³ | |
|
Polimeri Europa Extir® EH 5000 Expandable Polystyrene
Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | |
|
Polimeri Europa Extir® LN 2000 Expandable Polystyrene
Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 091 WU 80 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 092 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 642 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Density | 0.0170 - 0.0300 g/cc | 0.000614 - 0.00108 lb/in³ | Density range normally used |
|
Polimeri Europa Extir® A 2000 Expandable Polystyrene, Standard
(discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 16 g/l.Processing technology used for Type A 2000 is: Molding, Traditional.Specific characteristics..
|
|||
| Density | <= 0.0170 g/cc | <= 0.000614 lb/in³ | TMA |
|
Akzo Nobel Expancel® 054 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||