Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0200 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Density range normally used
Polimeri Europa Extir® B 2000 AE Expandable Polystyrene, Fast Molding Flame Retardant
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type B 2000 AE is: Molding, Vacuum.Specific characteristics: ..
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 140R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 150F Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 240R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 250R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0200 - 0.100 g/cc
0.000723 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 250R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS 33MC Modified Expandable Polystyrene
Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals.
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS 34RC Regular Expandable Polystyrene
Applications: PackagingInformation provided by NOVA Chemicals.
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Batch Expansion
NOVA Chemicals EPS M97C Expandable Polystyrene Resin
Applications Insulation, SIP's, ICF's, Fabricated PackagingInformation provided by NOVA Chemicals
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 35C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 45C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Density >= 0.0200 g/cc
>= 0.000723 lb/in³
Minimum apparent density on a continuous pre-expander after one expansion
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene  (discontinued **)
Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 422 FC Expandable Polystyrene
TPC - 422 FCApplications: shape molding of 6-10mm wall thicknessInformation provided by Iran Petrochemical Commercial Co.
Density 0.0200 g/cc
0.000723 lb/in³
0.9 minute residence time pre-expander
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
Density 0.0200 g/cc
0.000723 lb/in³
1.1 minute residence time pre-expander
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
Density 0.0200 g/cc
0.000723 lb/in³
110 second cycle time
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a..
Density 0.0200 g/cc
0.000723 lb/in³
125 rpm
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a..
Density 0.0200 - 0.0280 g/cc
0.000723 - 0.00101 lb/in³
sheet density
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0200 - 0.0270 g/cc
0.000723 - 0.000975 lb/in³
sheet density
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam
Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi..
Density 0.0200 g/cc
0.000723 lb/in³
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Density <= 0.0200 g/cc
<= 0.000723 lb/in³
TMA
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0200 g/cc
<= 0.000723 lb/in³
TMA
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0200 g/cc
<= 0.000723 lb/in³
TMA
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0200 g/cc
<= 0.000723 lb/in³
TMA
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0200 g/cc
0.000723 lb/in³
ISO 845
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Density 0.0200 - 0.0300 g/cc
0.000723 - 0.00108 lb/in³
molding density range
IRPC Polimaxx Pentfoam 422F Expandable Polystyrene
GENERAL: PENTFOAM "422F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
Density 0.0200 g/cc
0.000723 lb/in³
120 rpm
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Normal molded density
NOVA Chemicals Styrocell® D733A Expandable Polystyrene &nbsp;(discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 426 WP Expandable Polystyrene
TPC - 426 WPApplications: very low water absorption, cycling shape molding of 6-10 mm wall thicknessInformation provided by Iran Petrochemical Commercial Co.
Copyright © lookpolymers.com All Rights Reserved