Physical Properties Metric English Comments
Density 0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® A 5000 AE Expandable Polystyrene, Standard Flame Retardant
Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 10 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type ..
Density 0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® A 7000 AE Expandable Polystyrene, Standard Flame Retardant
Particle size range is 1.5 - 2.2 mm. Minimum apparent density after two expansions is 10 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l.Processing technology used for Type ..
Density 0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant
b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does..
Density 0.0150 - 0.0200 g/cc
0.000542 - 0.000723 lb/in³
Normal range, one pre-expansion
SABIC EPS 760FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 760FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Density 0.0150 - 0.0200 g/cc
0.000542 - 0.000723 lb/in³
Normal range, one pre-expansion
SABIC EPS 763 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 763 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 65D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of average and low densities.Information provided by NOVA Chemicals.
Density 0.0150 - 0.0200 g/cc
0.000542 - 0.000723 lb/in³
Pressurized batch pre-foamer; Usual Use
NOVA Chemicals Gedexcel® 74XA Expandable Polystyrene
Styrene homopolymer containing pentane, sued as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informatio..
Density 0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
Polimeri Europa Extir® LN 2001 Expandable Polystyrene
Extir LN 2001 belongs to a new expandable product family, the Leonardo Series. Extir LN 2001 is specially coated to be incorporated into bricks, concrete, mortar and plaster, in order to lighten the..
Density 0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene  (discontinued **)
Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Density 0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene  (discontinued **)
Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7..
Density 0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® A 2000/1 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density after two expansions is 12 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l. Minimum apparent density on a con..
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® IA 7000 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 1.4 - 2.2 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l.Processing technology used for Type I..
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T443B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Density 0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
molding density range
IRPC Polimaxx Pentfoam 155E Expandable Polystyrene
General: Pentfoam 155E is a self extinguising grad expandable polystyrene containing pentate as blowing agentApplications: Pentfoam 155E is particularly well suited for the manufacture of low densit..
Density 0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
molding density range
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene
General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..
Density 0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
molding density range
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene
General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar..
Density 0.0120 - 0.0200 g/cc
0.000434 - 0.000723 lb/in³
expanded
Jackon JACKOCELL® R212 Expanded Polystyrene Construction and Block Molding
High quality processingHigh strengthLow wasteFast moulding cycles
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® IA 5000 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.8 - 1.5 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l.Processing technology used for Type I..
Density 0.0180 - 0.0200 g/cc
0.000650 - 0.000723 lb/in³
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene
GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
Density 0.0180 - 0.0200 g/cc
0.000650 - 0.000723 lb/in³
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene
GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA..