Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0314 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792-91
Multibase Multi-Flex® TPO 4107 BLK
Data provided by Multibase.
Density 0.870 g/cc
0.0314 lb/in³
d20/20
Mitsui UNISTOLEâ„¢ P-401A Polyolefinic Primer/ Adhesive
UNISTOLEâ„¢ P is a liquid primer for coating and bonding polypropylene (PP) and various engineering plastics, rubber and other materials, which do not readily bond. Characteristics An easily han..
Density 0.870 g/cc
0.0314 lb/in³
ASTM D-792
Polyram BondyRam® 7001 Maleic Anhydride Modified Semi-crystalline EPDM Impact Modifier
Maleic Anhydride Modified Semi-crystalline EPDM recommended as impact modifier for polyamide compounds.Information provided by Polyram Ram On Ind.
Density 0.870 g/cc

@Temperature 15.6 °C
0.0314 lb/in³

@Temperature 60.1 °F
ASTM D4052
ExxonMobil 1000 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Density 0.870 g/cc

@Temperature 15.6 °C
0.0314 lb/in³

@Temperature 60.1 °F
ASTM D4052
ExxonMobil 220 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792, ISO 1183
DuPont™ Fusabond® N493 Polymer Modifier
DuPont™ Fusabond® N493 is an anhydride modified ethylene copolymer. DuPont™ Fusabond® N493 can only be used in the following applications: all polyamide blends and blends for golf balls and ble..
Density 0.870 g/cc
0.0314 lb/in³
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Density 0.869 g/cc

@Temperature 15.0 °C
0.0314 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil 32 Mobil EAL Envirosyn H Series
Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper..
Density 0.870 g/cc
0.0314 lb/in³
Dow AFFINITY™ EG 8100 Polyolefin Elastomer
AFFINITY® EG 8100 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation It ex..
Density 0.870 g/cc
0.0314 lb/in³
Dow AFFINITY™ EP 8500 Polyolefin Elastomer
AFFINITY® EP 8500 polyolefin elastomer is a saturated ethylene-octene copolymer for clear extruded profiles and tubing applications. It exhibits excellent clarity, elasticity and flexibility for lo..
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)
AFFINITY™ GA 1900 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and..
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Dow Engage® 8107 Polyolefin Elastomer
Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Dow Engage® 8207 Polyolefin Elastomer
Description: Engage® 8207 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Dow Engage® 8400 Polyolefin Elastomer
Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr..
Density 0.870 g/cc
0.0314 lb/in³
ConocoPhillips 100 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Density 0.870 g/cc
0.0314 lb/in³
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
Density 0.869 g/cc
0.0314 lb/in³
ConocoPhillips Hydroclear® 68 Multipurpose R&O Oil, AGMA Lubricant No. 2
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear ..
Density 0.870 g/cc
0.0314 lb/in³
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Supreme
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci..
Density 0.870 g/cc
0.0314 lb/in³
ConocoPhillips Hydroclear® El Mar® 15W-40 Low Ash Heavy Duty
Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du..
Density 0.869 g/cc
0.0314 lb/in³
ConocoPhillips Hydroclear® MV46 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Density 0.870 g/cc
0.0314 lb/in³
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer
ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materials.ChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and..
Density 0.869 g/cc
0.0314 lb/in³
ConocoPhillips Hydroclear Diamond Class® 100 Turbine Oil
Description: Conoco Hydroclear Diamond Class Turbine Oil is an extended service life rust- and oxidation-inhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Di..
Density 0.870 - 1.86 g/cc
0.0314 - 0.0672 lb/in³
Average value: 0.933 g/cc Grade Count:98
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Density 0.868 - 0.881 g/cc

@Temperature 15.0 °C
0.0314 - 0.0318 lb/in³

@Temperature 59.0 °F
Unipetrol Heavy Stabilized Oil Hydrogenate
Stabilized oil hydrogenates are a fraction boiling above approximately 250°C, obtained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of..
Copyright © lookpolymers.com All Rights Reserved