| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792-91 |
|
Multibase Multi-Pro® 0112 Black Polypropylene
Multi-Pro 0112 is a nucleated and antistated polypropylene homopolymer. It is designed for injection molding applications that require superior mold release properties.Data provided by Multibase.
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
PolyMirae Moplen HF550K Stretch/Yarn, Monofilament Grade Polypropylene
Moplen HF550K is the ADDIFORM polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Its appearance is spherical, white particle with diameter of 1mm ..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene
Moplen HP552R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552R is a homopolymer typically used by customers in high speed p..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
PolyMirae Moplen HP620M CPP Film Grade Polypropylene
Moplen HP620M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP620M is suitable for rigid core resin of CPP. Moplen HP620M res..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
PolyMirae Moplen RP344R Injection Molding Grade Polypropylene
Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Pinnacle Polymers 1512 Polypropylene Homopolymer, Fiber Spinning Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
|
|||
| Density | 0.900 - 1.18 g/cc | 0.0325 - 0.0426 lb/in³ | Average value: 0.994 g/cc Grade Count:32 |
|
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
PolyMirae Moplen HP425J BDDP Film Grade Polypropylene
Moplen HP425J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. MIRAEPOL T28C is a homopolymer particularly suitable for BOPP (Tender) fil..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Flint Hills 23T2A Random Copolymer Polypropylene
Features: Clarified, autoclave and good impact strength. Product does not contain animal derived components.Applications: Designed for Blow molding and ThermoformingInformation provided by Flint H..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Flint Hills 44S2A Polypropylene Impact Copolymer
Features: Phosphorus free additive package for silicon coated applications. Product does not contain animal derived components.Applications: Extrusion: blown and cast filmInformation Provided by Fl..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Flint Hills AP5106-HA Polypropylene Impact Copolymer
Features: Excellent impact stiffness balance, good mold release.Applications: Compression and injection molding: caps and closuresInformation Provided by Flint Hills Resources
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
|
Iran Petrochemical (PCC) EP2 X 49 GA Polypropylene
This grade features extremely high flow properties, excellent transparency and high gloss.Applications: Crouse holds containers, video cassette boxes, packaging for food, cosmetics.Information provi..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
|
Borealis BB108E Polypropylene compound for Steel Pipe Coating
BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG
|
|||
| Density | 0.900 - 0.910 g/cc | 0.0325 - 0.0329 lb/in³ | ISO 1183 |
|
Borealis RD734CF Polypropylene Random Copolymer
RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati..
|
|||
| Density |
0.900
g/cc @Temperature 15.6 °C |
0.0325
lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
|
ExxonMobil 32 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
|
|||
| Density |
0.899
g/cc @Temperature 15.6 °C |
0.0325
lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
|
ExxonMobil Mobil Almo 527
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene
Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Formosa Plastics Formolene® 6600A Impact Copolymer Polypropylene
Impact Copolymer for Extrusion and Compounding Applications (Fractional Melt Flow) Formolene® 6600A is a high impact copolymer with an excellent balance of toughness and stiffness. It is suitable f..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792, ISO 1183 |
|
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ExxonMobil Method |
|
ExxonMobil PP1013H1 Polypropylene Homopolymer
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ExxonMobil Method |
|
ExxonMobil PP1055E2 Polypropylene Homopolymer
Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
|
ExxonMobil PP4712E1 Polymer Grade for Oriented Film
Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ExxonMobil Method |
|
ExxonMobil PP7414 Polypropylene Homopolymer
Product Description: A medium impact strength copolymer resin designed for injection-molded automotive applications requiring medium melt flow rate.Availability: North America Features:Impact Modif..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
|
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow
This product is intended for thin-wall injection molding applications as well as low denier filament yarns, extrusion coating and specialty cast embossed film.Information provided by Entec
|
|||
| Density |
0.900
g/cc @Temperature 15.6 °C |
0.0325
lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
|
ExxonMobil 34 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
|
Dow INSPIRE™ 112 Performance Polymer
INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
|
Diamond Polymers NPP20-0201 Random Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
|
Arkema Group OREVAC® 18707 Grafted Maleic Anhydride Polypropylene
OREVAC 18707 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18707 ..
|
|||
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
|
Aclo Accucomp Polypropylene CPO407L Copolymer |
|||