| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
|
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
|
SABIC PP 518A Polypropylene Homopolymer for Fiber Applications
Product Description: PP 518A is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518A has the following features:Consistent processabilityGoo..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
|
Network Polymers NPP 25-3701
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D4883 |
|
Ineos H03W-01 Polypropylene, Gas Phase Polymerized
H03W-01 (formerly Fortilene® HG3253) belongs to the new generation of polypropylenes produced by gas phase polymerization. This nominal 4 melt flow index product is specifically designed for fib..
|
|||
| Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
|
Multibase Multi-Flex® TPE A 6001 BLK
TPE A 6001 is designed for gasket seals, rotational valves, and electrical applications as well as low friction applications. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis BC142MO Polypropylene Copolymer
BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. ..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis BD310MO Polypropylene Copolymer
BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis Borseal™ RE939CF Polypropylene Copolymer
Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging,..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding
Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis HK030U Polypropylene Compound
HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit..
|
|||
| Density | 0.906 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis RG460MO Polypropylene, Transparent Random Copolymer
RG460MO is a specially modified transparent polypropylene random copolymer with high melt flow. and is designed for high-speed injection molding and contains nucleating and demolding additives. Pro..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
|
Total PPC 4624WZ Polypropylene, Impact Copolymer
ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPC 5660 Propylene, Heterophasic Copolymer
ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
|
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Injection molding homopolymerNucleation - FINA 3620WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi- cavity molds.Antistat - FINA 3620WZ con..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
|
Total PPH 3727WZ Polypropylene, Injection Molding Grade
Fina’s new HIGH PERFORMANCE injection molding gradeBalanced Properties - Fina 3727WZ strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPH 4042 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance ..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPH 4060 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPH 9059 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 9059 is homopolymer.ApplicationATOFINA Polypropylene PPH 9059 is intended for extrusion of bulk continuous filament (BCF) and continuous filament (CF) fibers. PPH 9059 has..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis Bormod™ BF970MO Polypropylene for Injection Molding
Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Borealis RA130E-2492 Polypropylene Random Copolymer
RA130E-2492 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is dark blue colored. Applications: domestic water, heating, relining, plumbing, and in..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPC 2660 Polypropylene, Heterophasic Copolymer
ATOFINA Polypropylene PPC 2660 is a heterophasic copolymer. PPC 2660 is characterized by a low fluidity hence good melt strength to provide ease of processing and good manufactured article properti..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPC 3640 Polypropylene, Heterophasic Copolymer
ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPC 4660 Polypropylene, Heterophasic Copolymer
ATOFINA Polypropylene PPC 4660 is heterophasic copolymer.
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPC 4663 Polypropylene, Heterophasic Copolymer
ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou..
|
|||
| Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
|
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM-D792 |
|
Braskem PH 0130 HOMO Polypropylene Homopolymer
PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/im..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792A |
|
Braskem CP 144 Coating Polypropylene
Information provided by Braskem
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM-D792 |
|
Braskem PH 0950 HOMO Polypropylene Homopolymer
PH 0950 is a medium melt flow rate homopolymer with an antiblocking agent. PH 0950 is specially designed for twisted films produced by cast or blown film extrusion. It exhibits excellent optical pro..
|
|||
| Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D1505 |
|
Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
Bapolene PP4022 is a PP homopolymer designed for oriented film applications. It offers good clarity and optical properties. This resin meets FDA standards for food contact applications.Application..
|
|||
| Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
|
Total PPC 10712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage.
|
|||