| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | <= 0.930 g/cc | <= 0.0336 lb/in³ | ISO 1183 |
|
Murtfeldt Original Material ”S”® Natural Polyethylene
Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® natural has excell..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | STN 64 0111 |
|
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
|
Mytex Polymers AN16L(W)-D56 Polypropylene, Talc filled, Compounded, Elastomer, Impact modified
Description: AN16L-D56 is a compounded talc filled elastomer modified polypropylene with good impact and excellent material flow properties.Key Applications: Automotive exteriorInformation provided ..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183-A |
|
Okulen® 2000 PE-UHMW, SL
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
|
Polymer Industries Polyslick UHMW Rod
Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183-A |
|
Okulen® 2000 PE-UHMW, OF
OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | |
|
Mitsui Fybrel® UL 415 Polyolefin Synthetic Pulp, Dry Processes
(discontinued **)
Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type ..
|
|||
| Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D1505 |
|
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **)
Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D1505 |
|
Huntsman PE1651 EVA Film Extrusion
(discontinued **)
6.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with outstanding low temperature strength, excellent clarity, and good heat seal.Applications: Film extrusion: ice bags, liqui..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | Not Compounded |
|
KKPC KOSYN 1500NF Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D1505 |
|
Lushan VB150 Adhesive Resin for Aluminum-Plastic Composite Panel (ACP)
Adhesive resin Lushan series for Aluminum-plastic Composite Panel (ACP) proved required bonding strength between aluminum and the filled polyethylene core. The sandwich structure of Aluminum-plastic..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D1505 |
|
Lushan VB760 Adhesive Resin for Aluminum-Plastic Composite Panel (ACP), Mid Temperature
Adhesive resin Lushan series for Aluminum-plastic Composite Panel (ACP) proved required bonding strength between aluminum and the filled polyethylene core. The sandwich structure of Aluminum-plastic..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792B |
|
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant
Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processabilityApplications: furniture, small..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
|
Stellarchem SV-B40D TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | |
|
Styron Buna® SB 1723 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Composition: Buna® SB 1723 – Schkopau is manufactured by cold polymerization using mixed rosin acid /fatty acid soaps. In relation to solid rubber it is plasticized with 37.5 parts of TDAE o..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183B |
|
Styron INSPIREâ„¢ TF0808S(U) Polypropylene
TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE ..
|
|||
| Density | 0.929 g/cc | 0.0336 lb/in³ | ISO 1183 |
|
Borealis Himod™ FT7294 LDPE for Film
Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792, ISO 1183 |
|
DuPont Elvax® 3134SBZ Ethylene Vinyl Acetate
DuPont™ Elvax® 3134SBZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additiv..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D1505 |
|
UBE UBEPOL BR153A Oil-Extended Synthetic Rubber (Raw Polymer)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products. Stabilizer Type: StainingMicrostructure: cis: 98trans: 1vinyl: 1Information provided by UBE.
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792, ISO 1183 |
|
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid
Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | |
|
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | |
|
Dow LDPE 768A Low Density Polyethylene, Film Grade
DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | |
|
Dow SiLK™ Y 80 Semiconductor Dielectric Resin
SiLK™ Y 80 has an average pore size of < 2nm and a range of 1-3 nm, porous SiLK™ resins enables continuous Tantulum PVD barriers for 65 nm technology and beyond. Information provided by Dow
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792, ISO 1183 |
|
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | |
|
BASF Procom® X5S 770 Polypropylene
Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF.
|
|||
| Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
|
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures
PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as..
|
|||
| Density | 0.930 - 1.04 g/cc | 0.0336 - 0.0376 lb/in³ | Average value: 0.957 g/cc Grade Count:16 |
|
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..
|
|||