| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
|
Multibase Multi-Pro® 0612 CW Polypropylene
Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183-A |
|
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 - ISO 1183 |
|
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **)
Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
|
|||
| Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
|
ExxonMobil ESCOR™ AT 310 Extrusion Coating Resin
(discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
|
DuPont™ Surlyn® 8120 Ionomer Resin, Sodium
(discontinued **)
Surlyn® 8120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | Estimated by MatWeb |
|
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
(discontinued **)
Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
|
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade
PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 2781 |
|
KKPC KOSYN KTR 201 Thermoplastic Elastomer (TPE)
Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics ..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
|
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer
A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | Base Resin; ASTM D1505 |
|
Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding
Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides ..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
|
Borealis Borecene™ RM8402 Linear Polyethylene for Rotational Molding
Borecene RM8402 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
|
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating
9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to ..
|
|||
| Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D 792 |
|
Total 3802 Blue MDPE pipe, injection molding
FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
|
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength..
|
|||
| Density | 0.942 g/cc | 0.0340 lb/in³ | ASTM D4883 |
|
Westlake Tymax™ GA7501 Anhydride Modified Acrylate Copolymer (Developmental)
Westlake GA7501 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications wh..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D 792 |
|
Total 3802 YCF MDPE pipe grade
FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi..
|
|||
| Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
|
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
|
DuPont™ Bynel® 22E757 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | |
|
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
|
|||
| Density | 0.942 g/cc | 0.0340 lb/in³ | Exxon Method |
|
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate
Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer. TC 110 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact s..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
|
DuPont™ Surlyn® 1901 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1901 is a sodium ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultr..
|
|||
| Density |
0.940
g/cc @Temperature 23.0 °C |
0.0340
lb/in³ @Temperature 73.4 °F |
ISO 1183 |
|
Arkema Group LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
LOTRYL® Bestpeel 2407 is a ready-to-use thermoplastic composition designed to make peelable heat seal layers onto various substrates. The base resin is a random copolymer of ethylene and methyl acr..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM-D1505 / ASTM-D792 |
|
Braskem Evateno® 8019 PE EVA Foam Copolymer
The Evateno® 8019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium Vinyl-Acetate content. Evateno® 8019 PE is an easy processing and crosslinkable product with high compatibility with..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 2781 |
|
Alliance Polymers Viprene™ P45D-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P45D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Density |
0.940
g/cc @Temperature 23.0 °C |
0.0340
lb/in³ @Temperature 73.4 °F |
ISO 1183 |
|
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline ..
|
|||
| Density |
0.940
g/cc @Temperature 23.0 °C |
0.0340
lb/in³ @Temperature 73.4 °F |
ISO 1183 |
|
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam..
|
|||
| Density |
0.940
g/cc @Temperature 23.0 °C |
0.0340
lb/in³ @Temperature 73.4 °F |
ISO 1183 |
|
Arkema Group LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
LOTADER® AX 8900 is a random terpolymer of ethylene, acrylic ester and glycidyl methacrylate, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properti..
|
|||
| Density | 0.942 g/cc | 0.0340 lb/in³ | Exxon Method |
|
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula..
|
|||
| Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
|
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
|
|||
| Density | 0.942 g/cc | 0.0340 lb/in³ | Base Resin; ASTM D792 |
|
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables
Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by..
|
|||