| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant For those producing flammable materials and in the mining industry, explosion and fire are major dangers. It is of vital importance that in conveyor belts and bunkers, lining material is flame retar.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ISO 1183 |
| SABIC P5510 Black High Density Polyethylene for Pipes Product Description: P5510 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D 792 |
| NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolo.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | |
| Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips Marlex® HMN 55180 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product disp.. |
|||
| Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Formosa Plastics Formolene® DB5305A Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Polyethylene Formolene® DB5305A is tailored for large part blow molding applications. Besides having excellent chemical resistance properties Formolene® DB5305A HDPE ha.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Global G-2855 High Density Polyethylene, Blow Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Global N-3260 High Density Polyethylene, Yarn/Monofilament Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global .. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Reliance Industries Relene F56003 Polyethylene Relene F56003 is a High Density Polyethylene grade suitable for producing blown parts with excellent drawdown and paper like feel. It is recommended for making carrier bags and coextruded film stru.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| LyondellBasell Alathon® M5562 High Density Polyethylene ApplicationsALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include noz.. |
|||
| Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 µm) .. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing net, wire & cable insulators, auto parts, pipesMeets FDA requirements as listed.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Techmer ES HiFill® HDPE UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | Base Resin; ISO 1183 |
| Borealis BorPEX™ HE2558 Blue High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2558 is a blue, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long stability and UV resistance is ensured.. |
|||
| Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Borealis Borstar® MB7541 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce.. |
|||
| Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D792, ISO 1183 |
| DuPont™ Fusabond® E100 Polymer Modifier DuPont™ Fusabond® E100 is an anhydride modified high density polyethylene, mainly intended for use as a component in a blend with other polymers including polyolefins and polyamides. It is not int.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, .. |
|||
| Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| ExxonMobil HDPE HMA 018 High Density Polyethylene Resin Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Entec Hypel® PEHD18/.956 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
| Density | 0.954 g/cc | 0.0345 lb/in³ | Natural resin extruded under proper conditions with black masterbatch DFNF-0092 (6.5%); ASTM D792 |
| Dow DGDB-2480 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Su.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | |
| Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM-D792 |
| Braskem GM8250T HDPE High Density Extrusion Polyethylene GM8250T is a high-density polyethylene specially developed for the manufacturing of corrugated pipes. It has high molar mass and shows excellent tenacity, high stiffness, good impact resistance, and.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | |
| BASF Methyl Acrylate Formula: C4H6O2CAS: 96-33-3Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Methyl acrylate forms homopolymers and copolymers. Copolymer.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Polymer Industries Densetec HDPE TredSafe Board Designed specifically for the Playground and Marine industries, TredSafe incorporates the latest available technologies to produce a non-skid surface ideal for all type of flooring applications.Info.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer PRIMATOP HDPE 002955 has a high melt strength, excellent stiffness, and excellent stress crack resistance. Applications include large part blow molding resin and sheet extrusion thermoforming.Former.. |
|||
| Density | 0.956 g/cc | 0.0345 lb/in³ | Exxon Method |
| ExxonMobil Escorene® UL-7840C EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||