Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0350 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® B 3000 AE Expandable Polystyrene, Fast Molding Flame Retardant
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 17 g/l.Processing technology used for Type B 3000 AE is: Molding, Vacuum.Specific characteristics: DIN..
Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
Normal range, one pre-expansion
SABIC EPS 452 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 452 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Density 0.0220 - 0.0350 g/cc
0.000795 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 35C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 45C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Density 0.0170 - 0.0350 g/cc
0.000614 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 55XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
Density 0.0170 - 0.0350 g/cc
0.000614 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C..
Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene  (discontinued **)
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad..
Density 0.0170 - 0.0350 g/cc
0.000614 - 0.00126 lb/in³
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene  (discontinued **)
Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30..
Density 0.0210 - 0.0350 g/cc
0.000759 - 0.00126 lb/in³
Polimeri Europa Extir® F 1111 Expandable Polystyrene  (discontinued **)
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont..
Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® B 3000 Expandable Polystyrene, Fast Molding  (discontinued **)
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 17 g/l.Processing technology used for Type B 3000 is: Molding, Vacuum.Specific characteristics: Good m..
Density 0.0190 - 0.0350 g/cc
0.000686 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® PD D 2000 AE Expandable Polystyrene, Fast Molding Flame Retardant  (discontinued **)&lt
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l. Minimum apparent density on a continuous pre-expander is 20 g/l.Processing technology used..
Density 0.0170 - 0.0350 g/cc
0.000614 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® PD D 3000 AE Expandable Polystyrene, Fast Molding Flame Retardant  (discontinued **)&lt
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 16 g/l. Minimum apparent density on a continuous pre-expander is 18 g/l.Processing technology used fo..
Density 0.0210 - 0.0350 g/cc
0.000759 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® PD F 1111 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.2 - 0.5 mm. Minimum apparent density on a discontinuous pre-expander is 20 g/l. Minimum apparent density on a continuous pre-expander is 24 g/l.Processing technology used ..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 422 FC Expandable Polystyrene
TPC - 422 FCApplications: shape molding of 6-10mm wall thicknessInformation provided by Iran Petrochemical Commercial Co.
Density 0.0250 - 0.0350 g/cc
0.000903 - 0.00126 lb/in³
sheet density
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0270 - 0.0350 g/cc
0.000975 - 0.00126 lb/in³
sheet density
Zotefoams Plastazote® LD33LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0350 g/cc
0.000686 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® C 3000 Expandable Polystyrene, Fast Molding  (discontinued **)
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l.Processing technology used for Type C 3000 is: Molding, Vacuum.Specific characteristics: High t..
Density 0.0270 - 0.0350 g/cc
0.000975 - 0.00126 lb/in³
sheet density
Zotefoams Plastazote® LD34 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
Normal range, one pre-expansion
SABIC EPS 450FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 450FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Density 0.0200 - 0.0350 g/cc
0.000723 - 0.00126 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 426 WP Expandable Polystyrene
TPC - 426 WPApplications: very low water absorption, cycling shape molding of 6-10 mm wall thicknessInformation provided by Iran Petrochemical Commercial Co.