| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant
FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour sc..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | STN 64 0111 |
|
Plastcom SLOVALEN PH 49 GF 50 Polypropylene Homopolymer, 50% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 50% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East)
CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
|
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
Premix Thermoplastics PREFLEX E50 Polyphenylene Ether (PPO/PPE)
PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material ..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPC T16020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Density | 1.05 - 1.46 g/cc | 0.0379 - 0.0527 lb/in³ | Average value: 1.34 g/cc Grade Count:126 |
|
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
|
Global MPP-120-C 20% Mica Reinforced Polypropylene
Information provided by Global Polymers Corporation.
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
Meilian Chemical PE82085 BLUE MASTERBATCH
BLUE PE82085 is a blue LDPE based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Blue 15:1.Method of Usage: BLUE PE82085 is designed fo..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
Ineos ABS Lustran® LGA
Key Features:UnfilledSuitable processing methods:Injection molding
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
Momentive Performance Materials RTV102 White Adhesive Sealant, High Strength Paste
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
|
Lavergne VYSTYRENE PS 3904 High Impact Polystyrene
Vystyrene PS 3904 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
LyondellBasell Hostacomâ„¢ BG749GC/1 Polypropylene Copolymer
Description: Hostacomâ„¢ BG749GC/1 medium melt flow, 1,100 MPa flexural modulus, UV-stabilized, precolored, 20% calcium carbonate-filled polypropylene copolymer resin has an excellent combination..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Styrolution PS 456EB HIPS
Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yot.High fl..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Styrolution PS-145D Polystyrene
Description: Polystyrene 145D is a high flow, general purpose polystyrene. PS 145D offers exceptional processing characteristics for thing walled parts, multi-cavity tools, and complex designs. It i..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East)
NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required.
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned
Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D-792 |
|
Polyram BondyRam® 6000 Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene coupling agent
Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene recommended as coupling agent in Styrene composites with glass or other minerals.Information provided by Polyram Ram On Ind.
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | DIN 53479 |
|
Polyram PlusTek PB801 Nylon 6, Impact Modified
impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
ExxonMobil Exxtral™ HMU 210 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness for automotive HVAC and under-the-hood applications.Availability: Africa & Middle East, Asia Pacif..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Chi Mei Polylac® PA-756H ABS - High Flow
Super high flow
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
|
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
|
Ashley Polymers Ashlene® 940H Nylon 11
A general purpose highly flexible natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
A. Schulman ComAlloy Hiloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
|
Loctite® 569 Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
|
|||