| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
Multibase Multi-Pro® 2008 X Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO.1183 DIN.53479 |
|
Omnia Plastica ABS Acrylonitrile-butadiene-styrene
Acrylonitrile-butadiene-styrene is an amorphous thermopolymer used largely for injection moulded items. The stock shapes are mainly used for the production of prototypes.Features:Good machinability ..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
|
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792, ISO 1183 |
|
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPC 05ENH Polypropylene Copolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
|
Ineos ABS Centrex® 821 ASA Blend
(discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection ..
|
|||
| Density | 1.06 - 3.80 g/cc | 0.0383 - 0.137 lb/in³ | Average value: 1.42 g/cc Grade Count:323 |
|
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | DAM; ISO 1183 |
|
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
|
Momentive Performance Materials RTV1473 Black Adhesive Sealant, FIPG
One-part acetoxy cure. Typical uses: Heavy bodied adhesive sealant for formed-in-place gasketing. Good oil resistance.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | (DAM) |
|
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
|
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Carbon fiber. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
Techmer ES Elastoblend® PA6 IM L N
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc.
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
|
Suzhou Hipro Polymers Hiprolon® 90 NN Nylon 612, condition
Hiprolon® 90 NN is medium viscosity polyamide 6.12. Features: low density, low water absorption, high dimension stability, high impact and notched impact resistance, good chemical resistance and ..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM Data |
|
Dow Retain® ABS 7342 ABS
Data provided by Dow Chemical.
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
Buckeye Polymers BP ABS 6239 ABS
Very High HeatABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proce..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
BASF Ultramid® BU50I PA6 (Conditioned)
Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme ..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
|
3M Scotchkote™ FB856 Urethane Primer
Scotchkote Urethane Primer FB 856 has been specifically developed as a primer/sealer for porous mineral, timber and asphalt surfaces used on floors and roofs.Product Features:Combines good applicati..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | Uncured |
|
3M Scotch-Weld™ EC2500 General Purpose Instant Adhesive
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | |
|
Arkema Group Orgalloy® LE 6006 Nylon Alloy, 6% Glass Fiber Reinforced (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).6% glass fiber reinforced. Medium stiffness, good thermomechanical..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183A |
|
Ineos Nova 202 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **)
Excellent heat resistance, Fast cyclingApplications: XPS food packaging, Foam insulation, CD boxes, medical and food disposables, Sheet and profile extrusionProperties were determined on injection m..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
PolyOne Edgetek® MP-1000 Modified PPO - Unreinforced
(discontinued **)
Data provided by PolyOne.
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
|
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
|
|||
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
|
Polyram RamLloy PVB702 Nylon/ABS Alloy, Impact Modified
Impact modified, UV stabilized Nylon/ABS alloy for injection molding applications.Information provided by Polyram.
|
|||