| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | NCMT Method |
|
NCMT NanoPAC™ S205 High Performance Polypropylene Nanocomposite
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792B |
|
Dow INSPIRE™ TF2300 Thermoplastic Polyolefin
(discontinued **)
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792, ISO 1183 |
|
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | DAM; ASTM D792 |
|
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond)
Information provided by Ravago
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP CGI11 PS (Europe-Africa-Middle East)
LNP * Lubricomp* CGI11 is a compound based on Polystyrene resin containing Graphite. Added features include: Internally Lubricated.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
Ineos ABS Cadon® 127 SMA General Purpose, High Heat
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
Ineos ABS Lustran® H801
High heat resistance, PC modified, low emission, increased flow.,Property data per ISO test methods.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
|
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6
PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
|
LyondellBasell Hostacomâ„¢ GP622 Polypropylene Homopolymer
Description: Hostacomâ„¢ GP622 high melt flow, 2,900 MPa flexural modulus, 20% talc-filled polypropylene homopolymer is designed for high stiffness and excellent processability in thin-walled par..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | dry; ISO 1183 |
|
Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183/A |
|
Styron VELVEXâ„¢ 5250 SC Reinforced Elastomer/PP compound
Overview: VELVEXâ„¢ 5250 SC Natural is a reinforced elastomer/PP compound which provides a unique property balance of good stiffness, impact and high heat resistance in combination with a nice so..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled
SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate
SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
|
Borealis MS64T20 Polypropylene Compound, Mineral Filled
MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D 792 |
|
Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | dry; ISO 1183 |
|
DSM Novamid® ST120 NAT PA6-I
Impact Modified, Injection Molding
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
ExxonMobil Mytex™ AS65KW-LGDC
Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
Adell BD-30 Nylon 6, Ultra High Impact
Data provided by Adell Plastics, Inc.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
|
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
Aclo Accucomp SAN SAN900L |
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
|
DSM Akulon® K223-TP4 (Dry) Impact Modified Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | Sintered Part; ASTM D792 |
|
ALM FR 106 Nylon 11 SLS Prototyping Polymer
This flame retardant rapid prototyping material has additives in the raw material that allows it to pass aeronautic standard FAR25.853 smoke, flame, and toxicity tests. This material is ideal for Ae..
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific)
LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
|
|||