Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0390 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792-91
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene
Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled
Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group.
Density 1.08 g/cc
0.0390 lb/in³
NCMT Method
NCMT NanoPAC™ S206 High Performance Polypropylene Nanocomposite
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater..
Density 1.08 g/cc
0.0390 lb/in³
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Density 1.08 g/cc
0.0390 lb/in³
DIN 53479; ASTM D792
Kolon KOPA® KN333HI4 High Impact Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON CD0001 PS
LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Stat-kon CX01039 PS (Europe-Africa-Middle East)
LNP* Stat-kon* CX01039 is a compound based on Polystyrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Techmer ES Plastiblend® ABS 8015 CL
Availability: North AmericaForms: PelletsFeatures: CopolymerAppearance: Clear/TransparentInformation provided by TP Composites, Inc.
Density 1.08 g/cc
0.0390 lb/in³
Silon TA 2322 HD Blue Catalyst Masterbatch
Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2322 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System...
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Solvay TECHNYL® 27010ST PA66, Conditioned
Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of..
Density 1.08 g/cc
0.0390 lb/in³
DIN 53479
Polyram PlusTek PA860 Nylon 6.6, Impact Modified
Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.08 g/cc
0.0390 lb/in³
Loctite® 290 Wicking Grade Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Covestro Desmopan® W DP 89051D Polyurethane
PreprocessingMax. Water content
Density 1.08 g/cc

@Temperature 300 °C
0.0390 lb/in³

@Temperature 572 °F
Melt
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Ensinger Tecamid® ST Nylon (PA)
Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc.
Density 1.08 g/cc
0.0390 lb/in³
ASTM Data
Dow Tyril® 1000B SAN
TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good ..
Density 1.08 g/cc
0.0390 lb/in³
dry; ISO 1183
BASF Ultramid® 8255 HS PA6 (Conditioned)
Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and fle..
Density 1.08 g/cc
0.0390 lb/in³
Accelerator
3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives
3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and ..
Density 1.08 - 1.12 g/cc
0.0390 - 0.0405 lb/in³
ISO 1183
Austin Novel Materials Texalan® 465A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Ashley Polymers Ashlene® 827LD Nylon 6
A very high impact nylon resin for injection molding applications. Outstanding low temperature properties.Data provided by the manufacturer
Density 1.08 g/cc
0.0390 lb/in³
Solvay RHODAFAC® RA-600 E Surfactant
Description: Soluble in water and mineral oil. Exceptional stability in alkali. Outstanding compatibility in concentrated electrolyte solutions. Effective coupling agent for nonionic surfactants in ..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN
Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Styrolution Luran® 368 R SAN
General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Density 1.08 g/cc
0.0390 lb/in³
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled
SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
Density 1.08 g/cc
0.0390 lb/in³
Solvay RHODAFAC® RM-510 E Surfactant
Identification: POLYOXYETHYLENE DINONYLPHENYL ETHER PHOSPHATECAS: 39464 – 64 – 7Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, La..
Copyright © lookpolymers.com All Rights Reserved