Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0408 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
NYCOA 2025 Nylon 6
extrusion and molding grade with mold release and quicker cycle times for sports cleatsInformation provided by NYCOA, Inc.
Density 1.13 g/cc
0.0408 lb/in³
STN EN ISO 1183-1
Plastcom PLASTAMID® 66 BT N 27 B/IM PA66
PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, cla..
Density 1.13 g/cc
0.0408 lb/in³
STN 64 0111
Plastcom SLOVAMID 66 BT Polyamide 66
FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at low temperatures. Use in automotive, electrical, engineering and cons..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Nylene® 406F Nylon 6
Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Density 1.13 g/cc
<br>@Temperature 25.0 °C
0.0408 lb/in³
<br>@Temperature 77.0 °F
DSM Somos® 7110 Epoxy Photopolymer, Green Parts &nbsp;(discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Density 1.13 - 1.14 g/cc
0.0408 - 0.0412 lb/in³
Average value: 1.14 g/cc Grade Count:10
Overview of materials for Nylon 6 Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
BASF Capron® 8224 HSL Nylon 6 (DAM) &nbsp;(discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Density 1.13 g/cc
0.0408 lb/in³
ISO data
BASF Capron® 8202 NL Nylon 6 (Dry) &nbsp;(discontinued **)
Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Lanxess Durethan® C 38 FKAM 000000 Copolyamide
Copolyamide, film quality, high transparency, nucleated, high slip and lubricant content, medium-viscosity, good antiblock and dynamic slip propertiesApplication Examples: blown film coextrusion (ou..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Techmer ES HiFill® PA6 L N MB (Conditioned)
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region.
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific)
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Techmer ES Plastiblend® PC/ABS 830 SS7 BK
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Washington Penn Homopolymer Polypropylene 30% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D 792
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled
PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Density 1.13 g/cc
0.0408 lb/in³
Covestro Bayblend® T 64 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Covestro Bayblend® T65 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content
Density 1.13 g/cc
0.0408 lb/in³
dry; ISO 1183
DSM Akulon® F150-CZ PA6
Very High Viscosity, Lubricated
Density 1.13 g/cc
0.0408 lb/in³
Covestro Texin® 990 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792, ISO 1183
EPICHEM Epinyl PA 66 Polyamide 66
Density 1.13 g/cc
0.0408 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6 &nbsp;(Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO R 1184
Fainplast Compounds MPH 50/T Medical Flexible PVC, Extrusion
Technical tubes and peristaltic pump segments no DOP
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
BASF Ultramid® B33 01 PA6 (Dry)
Ultramid B33 01 is an intermediate viscosity. PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Covestro Bayblend® 2253 Polycarbonate + ABS Blend, Extrusion &nbsp;(discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with