| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
Plaskolite West Optix® CA-945 Clear Impact Modified Acrylic Resin
Impact modified acrylic resin, extrusion and injection moldingApplications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times ..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Description:0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubbe..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Polyether-based grades for film and sheet applications that require excellent resistance to hydrolysis and microbial attack.Information provided by Alliance Polymers
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
Multibase Multi-Flex® TPE A 6221 C BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | |
|
Taiwan Sheen Soon Sheenthane® A7530 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66
LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific)
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRILOY D2000I PC (Asia Pacific)
LNP* Lubriloy* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
Techmer ES HiFill FR® PA6/6 FR 144
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Halogen Free, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® HDPE GF30 CC 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing 30% Carbon Fiber. Added features of this material include: Clean Compounding System, Electrically Conductive...
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | Cured Resin |
|
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K
Fiber: AS7, Weave: UD, 134 g/m2Information provided by HexCel
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D 792 |
|
Cossa Polimeri ESTASTIR HI 0508 V0 Flame Retardant Polystyrene
Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
|
Covestro Desmopan® DP 9868DU Polyurethane
injection molding gradevery good hydrolysis and microbial resistancevery good low-temperature impact strengthopaqueCylindrical pelletsApplicationBoot shellsTechnical partsAs of 1 September 2015, Bay..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | (DAM); ISO 1183 |
|
DSM Akulon® K225-KS Nylon 6 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 55/K Flexible PVC, Lead Free
Inner tube
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183-1-A |
|
BASF Elastollan B 60 A ESD TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported)
Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat..
|
|||
| Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO 1183 |
|
Austin Novel Materials Texalan® 785A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon
Super Tough Nylon, Proprietary Filler(s),
|
|||
| Density | 1.17 g/cc | 0.0423 lb/in³ | |
|
Arkema Group Oroglas® MI-7T Acrylic
(discontinued **)
OROGLAS MI-7T is a medium impact grade combining excellent thermal resistance with good impact performance.Key features : impact resistance: up to 7 times more impact-resistant than standard acr..
|
|||