Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0430 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.18 - 1.19 g/cc
0.0426 - 0.0430 lb/in³
Polymerized; ASTM D792
Proto3000 Objet FullCure720 Transparent Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Density 1.18 - 1.19 g/cc
0.0426 - 0.0430 lb/in³
Polymerized; ASTM D792
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Density 1.04 - 1.19 g/cc
0.0376 - 0.0430 lb/in³
Average value: 1.05 g/cc Grade Count:99
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:17
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:11
Overview of materials for Acrylic, High Flow, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app..
Density 1.13 - 1.19 g/cc
0.0408 - 0.0430 lb/in³
Average value: 1.16 g/cc Grade Count:9
Overview of materials for Nylon, Barrier Film Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Barrier Film Copolymer". Each property range of values reported is minimum and maximum values of ..
Density 1.16 - 1.19 g/cc
0.0419 - 0.0430 lb/in³
Solvay GLOKILL® PQ60 Surfactant
Description: Algicide and biocide for swimming poolIdentification: POLYQUARTERNARY AMMONIUM CHLORIDE, AQUEOUS SOLUTIONCAS: 25988 – 97 – 0Available in: EuropeFunction: Algaecide for use in ..
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
ISO R 1183
Fainplast Compounds GS 30 Flexible PVC, Injection Molding, Lead Free
Scooter handle-bar grip
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
ISO R 1184
Fainplast Compounds MPH 57 Medical Flexible PVC, Extrusion
Tubolar apparatus and peristaltic pump segments
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
ISO R 1183
Fainplast Compounds PG 56/B Flexible PVC, Extrusion Modified with Rubber
Hydrocarbon resisting tubes
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
ISO R 1183
Fainplast Compounds PH 60/A Flexible PVC, Transparent Extrusion
Profiles, UL Class V2
Density 1.14 - 1.19 g/cc
0.0412 - 0.0430 lb/in³
Part A
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg..
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
ISO 1183
Austin Novel Materials Texalan® 564D Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Density 1.14 - 1.19 g/cc
0.0412 - 0.0430 lb/in³
Part A
3M Scotch-Weld™ DP600NS Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600NS is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a tri..
Density 1.14 - 1.19 g/cc
0.0412 - 0.0430 lb/in³
Part A
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Density 1.14 - 1.19 g/cc
0.0412 - 0.0430 lb/in³
Part A
3M Scotch-Weld™ DP601NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Density 0.913 - 1.19 g/cc
0.0330 - 0.0430 lb/in³
Average value: 0.940 g/cc Grade Count:29
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a..
Density 1.13 - 1.19 g/cc
0.0408 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:37
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Density 1.04 - 1.19 g/cc
0.0376 - 0.0430 lb/in³
Average value: 1.15 g/cc Grade Count:125
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Density 1.18 - 1.19 g/cc
0.0426 - 0.0430 lb/in³
Average value: 1.19 g/cc Grade Count:10
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:14
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..
Density 1.11 - 1.19 g/cc
0.0401 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:132
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..
Copyright © lookpolymers.com All Rights Reserved