| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 - 1.20 g/cc | 0.0426 - 0.0434 lb/in³ | ASTM D792 |
|
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing..
|
|||
| Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
|
Prodways PLASTCure Cast 200 3D Printing Polymer
Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar.
|
|||
| Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
|
Prodways PLASTCure Flex 100 3D Printing Polymer
High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for..
|
|||
| Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
|
Prodways PLASTCure Model 200 3D Printing Polymer
High temperature resistance.Thermoforming applicationsInformation provided by Genistar.
|
|||
| Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
|
Prodways PLASTCure Model 300 3D Printing Polymer
Good mechanical properties.Broad range of dental model applications.Information provided by Genistar.
|
|||
| Density | 1.02 - 1.20 g/cc | 0.0368 - 0.0434 lb/in³ | Average value: 1.05 g/cc Grade Count:101 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
|
|||
| Density | 1.19 - 1.20 g/cc | 0.0430 - 0.0434 lb/in³ | Average value: 1.20 g/cc Grade Count:17 |
|
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
|
|||
| Density | 0.700 - 1.20 g/cc | 0.0253 - 0.0434 lb/in³ | Average value: 1.17 g/cc Grade Count:249 |
|
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
|
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
|
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
|
Taiwan Sheen Soon Sheenthane® A8510H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
|
Taiwan Sheen Soon Sheenthane® A8521H TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
|
|||
| Density | 0.950 - 1.20 g/cc | 0.0343 - 0.0434 lb/in³ | Free flowing, Specification |
|
Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade)
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in..
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 58/O Flexible PVC, Injection Molding for Footwear
Antislip soles, opaque surface
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 59/T Flexible PVC, Injection Molding for Footwear
Crystal sandals
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 60/AS Flexible PVC, Injection Molding for Footwear
Oil resistent and antistatic soles
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 62/T Flexible PVC, Injection Molding for Footwear
Sandals
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 75/R1 Flexible PVC, Injection Molding for Footwear
Soles antiaccident shoes
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1184 |
|
Fainplast Compounds MPH 62/T Medical Flexible PVC, Extrusion
Technical tubes and peristaltic pump segments no DOP
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PG 55/A Flexible PVC, Extrusion Modified with Rubber
Gaskets modified with rubber
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PH 55 Flexible PVC, Transparent Extrusion
Transparent profiles
|
|||
| Density | 1.15 - 1.20 g/cc | 0.0415 - 0.0434 lb/in³ | |
|
BecauseWeCare BF90 Biodegradable Plastic
Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari..
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO 1183 |
|
Austin Novel Materials Texalan® 572D Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PMP 001/14 Flexible PVC, Extrusion Modified with PU
Various profiles
|
|||
| Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
|
Fainplast Compounds POLIFAIN 6020 Flexible PVC, Injection Molding for Footwear
Soles with PU
|
|||
| Density | 1.14 - 1.20 g/cc | 0.0412 - 0.0434 lb/in³ | Average value: 1.17 g/cc Grade Count:6 |
|
Overview of materials for Silicone Polyurethane, Polycarbonate Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim..
|
|||
| Density | 0.920 - 1.20 g/cc | 0.0332 - 0.0434 lb/in³ | Average value: 0.987 g/cc Grade Count:123 |
|
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
|
|||
| Density |
1.10
-
1.20
g/cc @Temperature 285 - 285 °C |
0.0397
-
0.0434
lb/in³ @Temperature 545 - 545 °F |
Average value: 1.19 g/cc Grade Count:27 |
|
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
|
|||
| Density | 0.950 - 1.20 g/cc | 0.0343 - 0.0434 lb/in³ | Average value: 1.13 g/cc Grade Count:94 |
|
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
|
|||
| Density | 0.970 - 1.20 g/cc | 0.0350 - 0.0434 lb/in³ | Average value: 1.12 g/cc Grade Count:8 |
|
Overview of materials for ABS/Polyurethane Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr..
|
|||