Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East)
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET  (Unverified Data**)
Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant
Information provided by Polykemi AB
Density 1.22 g/cc
0.0441 lb/in³
Injection molded parts; ASTM D792
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester
Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe..
Density 1.22 g/cc
<br>@Temperature 23.0 °C
0.0441 lb/in³
<br>@Temperature 73.4 °F
ISO 1183
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183/A
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled
Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DX05301C PC
LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC
LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s).
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific)
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys..
Density 1.22 g/cc
0.0441 lb/in³
DIN 53479
Polyram RamOfin PPH300J8 Polypropylene, 40% Glass Fiber
40% glass fiber and glass beads reinforced, high stiffness polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Covestro Desmopan® DP 3354D Polyurethane
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 1.22 g/cc
0.0441 lb/in³
Covestro Makroblend® UT-1018 Polycarbonate + Polyester Blend
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingSheet extrusionInformation provided by Bayer Polymers.As of 1 ..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
EMS-Grivory Grivory® LV-3H PA12-GF30
Product description: Grilamid LV-3H is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET &nbsp;(Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET &nbsp;(Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Density 1.22 g/cc
0.0441 lb/in³
Dow ISONATE™ 240 MDI Prepolymer
ISONATE™ 240 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with a high molecular weight polyester polyol, resulting in a material with good..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
DSM Arnite® B604T PBT-I
Density 1.22 g/cc
0.0441 lb/in³
ASTM D1505-79 (Mod. to DuPont method)
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge
Melinex® 487 is a high-yield, white film that is coated on one side for adhesion to inks, coatings, laser printing, and thermal transfer printing.Information provided by DuPont.
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey
Information provided by Eurotec®
Density 1.22 g/cc
0.0441 lb/in³
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric..
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
BASF Elastollan® S85A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..
Density 1.22 g/cc
0.0441 lb/in³
BASF Lupranate® MM103 Isocyanate Modified MDI
Description: Lupranate® MM103 is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate MM103 serves as the isocyanate component in the production of microcellular urethane el..
Density 1.22 g/cc
0.0441 lb/in³
B Component; ASTM D1475
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating
Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e..
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183-1-A
BASF Elastollan 890 AN TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Density 1.22 g/cc
0.0441 lb/in³
BASF Lupranate® 78 Isocyanate
Description: Lupranate® 78 Isocyanate is a polymeric MDI with a functionality of approximately 2.3. This product exhibits excellent low temperature stability. Lupranate 78 Isocyanate will remain a ..
Density 1.22 g/cc
0.0441 lb/in³
BASF Lupranate® M10 Isocyanate
Description: Lupranate® M10 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate M10 Isocyanate is a polymeric MDI which contains a relatively high level ..
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.